TECHNYL® A 218 Y10 NATURAL

Category: Nylon 66 , Polyamide 66
Manufacturer: Solvay Engineering Plastics
Trademark: TECHNYL®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: XkRs6N_TECHNYLA218Y10NATURAL.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
TECHNYL® A 218 Y10 is an unreinforced polyamide 66, medium viscosity, heat stabilized and specially modified to have improved frictionnal properties for injection moulding. This grade offers all of the primary properties of unreinforced polyamide 66 and mainly has excellent surface properties as low coefficient of friction and good resistance to wear.
General Information
Additive
  • heat stabilizer
Features
  • Heat Stabilized - Inorganic
  • Low friction coefficient
  • Excellent appearance
Uses
  • Large household appliances and small household appliances
  • Industrial application
  • Pulley
  • Consumer goods application field
Agency Ratings
  • EC 1907/2006 (REACH)
RoHS Compliance
  • RoHS compliance
Appearance
  • Dark gray
Forms
  • Particle
Processing Method
  • Injection molding
Multi-Point Data
  • Isothermal Stress vs. Strain (ISO 11403-1)
Resin ID (ISO 1043)
  • PA66
PhysicalDryConditionedUnitTest Method
Density 1.16--g/cm³ISO 1183/A
Water Absorption ISO 62
     23°C, 24 hr 1.2--%ISO 62
     Equilibrium, 23°C, 50% RH 2.8--%ISO 62
MechanicalDryConditionedUnitTest Method
Tensile Modulus (23°C)39001500MPaISO 527-2/1A
Tensile Stress ISO 527-2/1A
     Yield, 23°C 83.065.0MPaISO 527-2/1A
     Fracture, 23°C 92.043.0MPaISO 527-2/1A
Tensile Strain ISO 527-2
     Yield, 23°C 1022%ISO 527-2
     Fracture, 23°C 9.098%ISO 527-2
Flexural Modulus (23°C)29001300MPaISO 178
Flexural Stress (23°C)12565.0MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength (23°C)3.510kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength (23°C)No Break--ISO 179/1eU
Notched Izod Impact (23°C)3.58.0kJ/m²ISO 180
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature
     0.45 MPa, not annealed 230--°CISO 75-2/Bf
     1.8 MPa, not annealed 80.0--°CISO 75-2/Af
Melting Temperature 263--°CISO 11357-3
ElectricalDryConditionedUnitTest Method
Surface Resistivity 1.0E+141.0E+12ohmsIEC 60093
Volume Resistivity 1.0E+151.0E+13ohms·cmIEC 60093
Dielectric Strength (2.00 mm)3028kV/mmIEC 60243-1
Dissipation Factor 0.0200.11IEC 60250
Comparative Tracking Index (Solution A)575600VIEC 60112
FlammabilityDryConditionedUnitTest Method
Oxygen Index 26--%ISO 4589-2
InjectionDryUnit
Drying Temperature 80°C
Suggested Max Moisture 0.20%
Rear Temperature 265 - 275°C
Middle Temperature 270 - 280°C
Front Temperature 280 - 285°C
Mold Temperature 60 - 80°C
Injection instructions
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For unfilled polyamide, Solvay recommends the use of high alloy steel with a weak chromium content. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design
Resin Grade Manufacturer Category Trademark
Propafilm™ XLT65 Innovia Films Ltd. PP Alloy Propafilm™
Thermylene® P6-25FG-0687 Asahi Kasei Plastics North America Inc. PP, Unspecified Thermylene®
Westlake LDPE EM812AA Westlake Chemical Corporation LDPE Westlake LDPE
DINALON® B1S35 V2-7035 Grupo Repol Nylon 6 DINALON®
LNP™ LUBRICOMP™ ZX05506 compound SABIC Innovative Plastics PPE+PS LNP™ LUBRICOMP™