| Category: | TPV , Thermoplastic Vulcanizate |
| Manufacturer: | Riken Technos Corp. |
| Trademark: | Actymer® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | XfLKgm_Actymer-AE-2080S.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Actymer®AE-2080S is a thermoplastic vulcanized rubber (TPV) product,. It is available in North America or Asia Pacific. Features include:
|
| General Information | |
|---|---|
| Features |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.938 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 80 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (100% Strain) | 3.80 | MPa | ISO 37 |
| Tensile Stress (Yield) | 17.7 | MPa | ISO 37 |
| Tensile Elongation (Break) | 780 | % | ISO 37 |
| Tear Strength | 45 | kN/m | ISO 34-1 |
| Compression Set | ISO 815 | ||
| 70°C, 72 hr | 51 | % | ISO 815 |
| 120°C, 72 hr | 63 | % | ISO 815 |
| Aging | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Change in Tensile Strength in Air (136°C, 168 hr) | 0.0 | % | ISO 188 |
| Change in Tensile Strain at Break in Air (136°C, 168 hr) | 0.0 | % | ISO 188 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | -60.0 | °C | ISO 974 |
| Additional Information |
|---|
| The values listed above are tested in accordance with JIS K test methods.Rebound Resilience: 48% |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Rilsamid® ASR 13 | Arkema | Nylon 12 | Rilsamid® |
| RTP 203 B | RTP Company | Nylon 610 | RTP |
| RTP 100 SI 2 HF | RTP Company | PP Homopolymer | RTP |
| SCHULAMID® 612 GF 30 H9 | A. Schulman Europe | Nylon 612 | SCHULAMID® |
| Fiberfil® J-69/40/E | Fiberfil® Engineered Plastics Inc. | PP Homopolymer | Fiberfil® |