Message |
---|
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.36 | g/cm³ | ISO 1183 |
Water Absorption (Equilibrium, 23°C, 50% RH) | 1.3 | % | ISO 62 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 122 | ISO 2039-2 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 160 | MPa | ISO 527-2 |
Tensile Strain (Break) | 3.0 | % | ISO 527-2 |
Flexural Modulus | 8700 | MPa | ISO 178 |
Flexural Stress | 230 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 7.0 | kJ/m² | ISO 179/1eA |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, not annealed | 220 | °C | ISO 75-2/B |
1.8 MPa, not annealed | 210 | °C | ISO 75-2/A |
Melting Temperature 1 | 220 | °C | ISO 11357-3 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+15 | ohms·cm | IEC 60093 |
Relative Permittivity (1 MHz) | 3.80 | IEC 60250 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (0.8 mm) | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | |||
-- | 90 | °C | |
Dry Air Dryer | 80 | °C | |
Drying Time | |||
-- | 6.0 - 8.0 | hr | |
Dry Air Dryer | 4.0 - 6.0 | hr | |
Suggested Max Moisture | 0.050 | % | |
Hopper Temperature | 60 - 80 | °C | |
Rear Temperature | 250 | °C | |
Middle Temperature | 250 | °C | |
Front Temperature | 250 | °C | |
Nozzle Temperature | 260 | °C | |
Mold Temperature | 70 - 90 | °C | |
Back Pressure | 0.490 - 0.981 | MPa | |
Screw Speed | 80 - 120 | rpm |
Note Message | |
---|---|
1 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RAYPRENE® NB221-S4042 | R&P (Pte.) Ltd. | TPE | RAYPRENE® |
Kepex® 3300 | Korea Engineering Plastics Co., Ltd | PBT | Kepex® |
LEXAN™ CFR7630 resin | SABIC Innovative Plastics | PC | LEXAN™ |
Sylvin 8839-60D Grey 9506 | Sylvin Technologies Incorporated | PVC, Rigid | Sylvin |
Sylvin 9604-90 Grey 9225 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |