Therma-Tech™ TT9200-5003 EC MID Anthracite

Category: PPS , Polyphenylene Sulfide
Manufacturer: PolyOne Corporation
Trademark: Therma-Tech™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: X9Bt7V_Therma-Tech-TT9200-5003-EC-MID-Anthracite.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of thermoplastics. These materials provide the benefits of proprietary conductive additive technologies and the performance of select engineering thermoplastic resins. Therma-Tech compounds have been shown to improve thermal conductivity up to 100-times that of conventional plastics and can be used in a wide range of thermal management applications.
General Information
Filler / Reinforcement
  • Glass Fiber
Features
  • Electrically Conductive
  • Thermally Conductive
Uses
  • Automotive Applications
  • Automotive Under the Hood
  • Consumer Applications
  • Electrical/Electronic Applications
  • Housings
  • Industrial Applications
RoHS Compliance
  • RoHS Compliant
Forms
  • Pellets
Processing Method
  • Extrusion
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.78g/cm³ISO 1183
Molding Shrinkage - Flow (Injection Molded)0.20 to 0.40%ISO 294-4
MechanicalNominal ValueUnitTest Method
Tensile Modulus 117500MPaISO 527
Tensile Stress (Break)58.0MPaISO 527-2/1/50
Tensile Elongation 2(Break)0.30 to 0.50%ISO 527
Flexural Modulus 3(Injection Molded)13500MPaISO 178
Flexural Strength 4(Injection Molded)75.0MPaISO 178
ImpactNominal ValueUnitTest Method
Charpy Notched Impact Strength (23°C)2.3kJ/m²ISO 179
Charpy Unnotched Impact Strength (23°C)3.9kJ/m²ISO 179
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Annealed)260°CISO 75-2/A
Thermal Conductivity
    -- 52.2 to 2.6W/m/K
    -- 63.5 to 4.0W/m/KASTM E1461
    -- 716 to 18W/m/KASTM E1461
ElectricalNominal ValueUnitTest Method
Surface Resistivity < 1.0E+4ohmsIEC 60093
FlammabilityNominal ValueUnitTest Method
Flame Rating UL 94
    1.50 mm 5VA
    3.00 mm 5VA
Glow Wire Flammability Index IEC 60695-2-12
    0.800 mm 960°C
    1.60 mm 960°C
    3.00 mm > 960°C
Glow Wire Ignition Temperature (3.00 mm)> 960°CIEC 60695-2-13
InjectionNominal ValueUnit
Processing (Melt) Temp 310 to 340°C
Mold Temperature 140 to 170°C
Note Message
1 .Type I, 1.0 mm/min
2 .Type I, 50 mm/min
3 .10 mm/min
4 .10 mm/min
5 .Through Plane with Modified Transient Plane Source technique, C-Therm TCi™
6 .Through Plane
7 .In Plane
Resin Grade Manufacturer Category Trademark
Miramid® SEP15C BASF Leuna GmbH Nylon 66 Miramid®
NEXT REGRIND POMC M90-300RG NEXT Specialty Resins, Inc. Acetal (POM) Copolymer NEXT REGRIND
Network Polymers HDPE 50 0355 Network Polymers, Inc. HDPE Network Polymers HDPE
Chemlon® MDM54 Teknor Apex Company (Chem Polymer) Nylon 6 Chemlon®
GELOY™ XP7550 resin SABIC Innovative Plastics ASA+PC GELOY™