| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Nytex Composites Co., Ltd. |
| Trademark: | NYLOY® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | WidMq6_NYLOYNG0813B.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| NYLOY®NG-0813B is a polyamide 6 (nylon 6) material, which contains a 13% filler. This product is available in North America or Asia Pacific region. The processing method is injection molding. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.24 | g/cm³ | ASTM D792 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 88.1 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 2.0 | % | ASTM D638 |
| Flexural Modulus | 4900 | MPa | ASTM D790 |
| Flexural Strength | 132 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (3.18 mm) | 37 | J/m | ASTM D256 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 110 | °C | |
| Drying Time | 1.0 | hr | |
| Rear Temperature | 240 | °C | |
| Middle Temperature | 250 | °C | |
| Nozzle Temperature | 260 | °C | |
| Mold Temperature | 80 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Aaroprene® CFPP 2040 | Aaron Industries Corp. | PP, Unspecified | Aaroprene® |
| COPYLENE® CR350CL-02 | Phillips 66 | PP Random Copolymer | COPYLENE® |
| DELPET™ SR6200 | Asahi Kasei Chemicals Corporation | Acrylic (PMMA) | DELPET™ |
| Koylene SM250N | Reliance Industries Limited | PP Homopolymer | Koylene |
| Lifolit® SG 45.1095/1 NP | ELASTO | PVC, Flexible | Lifolit® |