| Category: | EVA , Ethylene Vinyl Acetate Copolymer |
| Manufacturer: | Celanese EVA Performance Polymers |
| Trademark: | Ateva® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | WgOPdE_Ateva-1641.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| This resin is well suited for extrusion coating, coextrusion and specialty lamination applications. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.936 | g/cm³ | ASTM D1505 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 28 | g/10 min | ASTM D1238 |
| Vinyl Acetate Content | 16.0 | wt% |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shore A | 90 | ||
| Shore D | 35 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength 1(Break) | 9.00 | MPa | ASTM D638 |
| Tensile Elongation 2(Break) | 700 | % | ASTM D638 |
| Flexural Modulus - 1% Secant | 60.0 | MPa | ASTM D790 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 62.0 | °C | ASTM D1525 |
| Peak Melting Temperature | 89.0 | °C | ASTM D3418 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Melt Temperature | < 210 | °C |
| Note Message | |
|---|---|
| 1 . | Type IV, 50 mm/min |
| 2 . | Type IV, 50 mm/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| PRL PC-G30-(color)-1 | Polymer Resources Ltd. | PC | PRL |
| METLBOND® 1515-3 | Cytec Industries Inc. | Epoxy | METLBOND® |
| SPESIN® KP213G15BL | Kolon Plastics, Inc. | PBT | SPESIN® |
| Jam PE 526F2 | Jam Petrochemical Company | HDPE | Jam PE |
| Lion Idemitsu Composites PPS K532P1 | Lion Idemitsu Composites Co., Ltd. | PPS | Lion Idemitsu Composites PPS |