Category: | PP Homopolymer , Polypropylene Homopolymer |
Manufacturer: | Safripol (PTY) LTD |
Trademark: | Safron® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | WZ4cpz_Safron-H510-02.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Safron® H510-02 Polypropylene Resin is a homopolymer suitable for extrusion, general purpose injection and blow moulding. It offers good processability and low water carry-over, required when water baths are used during processing. Safron® H510-02 Polypropylene Resin offers good tenacity and low fibrillation. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.900 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 2.0 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, Injection Molded) | 31.0 | MPa | ISO 527-2 |
Tensile Strain (Yield, Injection Molded) | 8.5 | % | ISO 527-2 |
Flexural Modulus (Injection Molded) | 1360 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C, Injection Molded) | 6.8 | kJ/m² | ISO 179/1eA |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, not annealed | 85.0 | °C | ISO 75-2/B |
1.8 MPa, not annealed | 53.0 | °C | ISO 75-2/A |
Vicat Softening Temperature 2 | 90.0 | °C | ISO 306/B |
Additional Information |
---|
Blow Molding conditions: Zone 1: 180 to 200°C Zone 2: 210 to 230°C Zone 3: 230 to 250°C Zone 4: 220 to 240°C Die: 220°C |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 190 | °C | |
Middle Temperature | 220 - 230 | °C | |
Front Temperature | 240 - 250 | °C | |
Nozzle Temperature | 240 | °C |
Injection instructions |
---|
Zone 4 Temperature: 245°C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 190 | °C | |
Cylinder Zone 2 Temp. | 215 | °C | |
Cylinder Zone 3 Temp. | 240 | °C | |
Cylinder Zone 4 Temp. | 250 | °C | |
Die Temperature | 245 | °C |
Note Message | |
---|---|
1 . | Injection Molded |
2 . | Injection Molded |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Styropor® BFL 395 | BASF Corporation | PS (EPS) | Styropor® |
TOTAL Polypropylene PPC 4820WZ | TOTAL Refining & Chemicals | PP Impact Copolymer | TOTAL Polypropylene |
Leona™ 1402SH | Asahi Kasei Chemicals Corporation | Nylon 66 | Leona™ |
Lucel® N109LD | LG Chem Ltd. | Acetal (POM) Copolymer | Lucel® |
Durethan® BKV 115 H3.0 DUS008 000000 | LANXESS GmbH | Nylon 6 | Durethan® |