Category: | TPO (POE) , Thermoplastic Polyolefin Elastomer |
Manufacturer: | KMI Group, Inc. |
Trademark: | Elastoprene |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | VGHeQr_ElastopreneHS5150DNAT.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Elastoprene HS5150D is a flexible TPE/TPO hybrid intended for injection molding applications, offering good processibility, easy coloring, good heat resistance, improved flexural fatigue and FDA compliance. Applications: Food containers, food closures, storage containers, general industrial and consumer goods applications. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.970 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 25 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw D, 10 seconds, extruded | 48 | ASTM D2240 | |
Shore D, 10 seconds, injection molding | 50 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 5.45 | MPa | ASTM D412 |
Tensile Strength (Break) | 15.3 | MPa | ASTM D412 |
Tensile Elongation (Break) | 600 | % | ASTM D412 |
Tear Strength | 74.0 | kN/m | ASTM D624 |
Compression Set | ASTM D395B | ||
23°C, 22 hr | 52 | % | ASTM D395B |
70°C, 22 hr | 71 | % | ASTM D395B |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -50.0 | °C | ASTM D746 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 171 - 199 | °C | |
Middle Temperature | 177 - 210 | °C | |
Front Temperature | 191 - 221 | °C | |
Nozzle Temperature | 199 - 229 | °C | |
Processing (Melt) Temp | 199 - 221 | °C | |
Mold Temperature | 10 - 49 | °C | |
Injection Pressure | 5.17 - 8.96 | MPa | |
Injection Rate | Fast | ||
Screw Speed | 50 - 200 | rpm | |
Clamp Tonnage | 2.8 - 4.8 | kN/cm² | |
Cushion | 5.08 - 12.7 | mm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SABIC® PPcompound 19T1040 | Saudi Basic Industries Corporation (SABIC) | PP Homopolymer | SABIC® PPcompound |
Chemlon® 235G | Teknor Apex Company (Chem Polymer) | Nylon 6 | Chemlon® |
DJSilicone NE-9360 | DONGJUE SILICONE (NANJING) CO., LTD | Silicone | DJSilicone |
ELASTOSIL® LR 3071/60 A/B | Wacker Chemie AG | Silicone | ELASTOSIL® LR |
Hostacom ERC 161N G22452 | LyondellBasell Industries | PP Copolymer | Hostacom |