Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | UxdXvK_TECHNYLA218V33BLACK51.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL® A 218 V33 Black 51 is a polyamide 66, reinforced with 33% of glass fibre, heat stabilized, for injection moulding. This grade offers an excellent combination between thermal and mechanical properties. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.39 | -- | g/cm³ | ISO 1183/A |
Water Absorption | ISO 62 | |||
23°C, 24 hr | 0.78 | -- | % | ISO 62 |
Saturated, 23°C | 5.5 | -- | % | ISO 62 |
Equilibrium, 23°C, 50% RH | 1.6 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 11300 | 7700 | MPa | ISO 527-2/1A |
Tensile Stress (Break, 23°C) | 200 | 135 | MPa | ISO 527-2/1A |
Tensile Strain (Break, 23°C) | 3.0 | 5.0 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 12 | 16 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 85 | 94 | kJ/m² | ISO 179/1eU |
Notched Izod Impact (23°C) | 13 | 17 | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 250 | -- | °C | ISO 75-2/Af |
Melting Temperature | 262 | -- | °C | ISO 11357-3 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 270 - 280 | °C | |
Middle Temperature | 275 - 285 | °C | |
Front Temperature | 280 - 290 | °C | |
Mold Temperature | 70 - 100 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 208A | RTP Company | Nylon 6 | RTP |
Ravago Compounds HMP-307M (Roto) | Ravago Manufacturing Americas, LLC | LLDPE | Ravago Compounds |
WELLAMID Nylon 6600 GV 20 HWCP | CP-Polymer-Technik GmbH & Co. KG | Nylon 66 | WELLAMID Nylon |
BioCeres® BC-LBF01 | FuturaMat | Biodeg Polymers | BioCeres® |
PALRAN® R S H 08 GF 16 | pal plast GmbH | ABS | PALRAN® |