Category: | MDPE , Medium Density Polyethylene |
Manufacturer: | Hanwha Chemical |
Trademark: | HANWHA |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Udlpbd_HANWHA-CMBA-8240BK.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Hanwha CMBA-8240BK is a black medium density polyethylene(MDPE) compound designed for power & communication cable jacketing applications. It combines excellent physical properties with good processing. It provides excellent resistance to environmental stress cracking(ESCR) and thermal oxidative degradation. It contains 2.5% well-dispersed carbon black to ensure excellent weathering resistance. |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.949 | g/cm³ | ASTM D1505 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 0.23 | g/10 min | ASTM D1238 |
Environmental Stress-Cracking Resistance (50°C, 10% Igepal, F0) | > 5000 | hr | ASTM D1693 |
Carbon Black Content | 2.5 | % | ASTM D1603 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D, 1 sec) | 59 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 29.4 | MPa | ASTM D638 |
Tensile Elongation (Break) | 800 | % | ASTM D638 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Oven Aging (100°C) | 10.0 | day | |
Tensile strength retention- 10 days (100°C) | > 85 | % | ASTM D638 |
Retention of Tensile Elongation - 10 days (100°C) | > 85 | % | ASTM D638 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Thermal Stress Crack Resistance | > 96 | hr | ASTM D2951 |
Oxygen sensing time- AI (200°C) | > 100 | min | ASTM D3895 |
Optical | Nominal Value | Unit | Test Method |
---|---|---|---|
Light Absorption Coefficient | > 400 | Abs/mm | ASTM D3349 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -76.0 | °C | ASTM D746 |
Electrical | Nominal Value | Test Method | |
---|---|---|---|
Dielectric Constant (1 MHz) | 2.40 | ASTM D150 | |
Dissipation Factor (1 MHz) | 5.0E-4 | ASTM D150 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 200 - 230 | °C |
Extrusion instructions |
---|
Hopper drying : 70°C/3hrs is recommended |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TPV Elastoprene® N64A-i | ELASTORSA Elastomeros Riojanos S.A. | PP+EPDM | TPV Elastoprene® |
AKROMID® B3 GM 15/15 natural (3079) | AKRO-PLASTIC GmbH | Nylon 6 | AKROMID® |
APEX® 65007 | Teknor Apex Company | PVC, Flexible | APEX® |
EcoLon® 2000-BK1 | Wellman Engineering Resins | Nylon 66 | EcoLon® |
Sylvin 8240-80FU White 1512 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |