Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | ResMart |
Trademark: | ResMart Repro |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | UYyZzk_ResMart-Repro-Nylon-6-6.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Reprocessed nylon 6 6 that provides an economical property set |
General Information | |
---|---|
Recycled Content |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.14 | g/cm³ | ASTM D792 |
Moisture Content | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 62.1 | MPa | ASTM D638 |
Tensile Elongation (Yield) | > 10 | % | ASTM D638 |
Flexural Modulus | 2690 | MPa | ASTM D790 |
Flexural Strength | 82.7 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 45 | J/m | ASTM D256 |
Unnotched Izod Impact (3.18 mm) | 1100 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (0.45 MPa, Unannealed) | 199 | °C | ASTM D648 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature - Desiccant Dryer | 82.2 | °C | |
Drying Time - Desiccant Dryer | 3.0 - 4.0 | hr | |
Suggested Max Moisture | 0.18 | % | |
Processing (Melt) Temp | 277 - 299 | °C | |
Mold Temperature | 48.9 - 90.6 | °C |
Injection instructions |
---|
Dew Point: 0°F |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 205 D HS TFE 15 | RTP Company | Nylon 612 | RTP |
TAROMID A 280 G5 Y0 | Taro Plast S.p.A. | Nylon 66 | TAROMID A |
NuSil MED-1511 | NuSil Technology | Silicone | NuSil |
Osterlene® HI-9-2.6-stg | Osterman & Company | PS (HIPS) | Osterlene® |
Sumiliteresin® PR-50087 | SBHPP | Phenolic | Sumiliteresin® |