Chemlon® 113 GX is a Polyamide 66 (Nylon 66) material filled with 13% glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding.

Important attributes of Chemlon® 113 GX are:
  • Flame Rated
  • Creep Resistant
  • Good Dimensional Stability
  • Good Stiffness
  • High Strength
General Information
Filler / Reinforcement
  • Glass Fiber, 13% Filler by Weight
Additive
  • Lubricant
Features
  • Good Creep Resistance
  • Good Dimensional Stability
  • Good Stiffness
  • High Tensile Strength
  • Lubricated
Appearance
  • Natural Color
Forms
  • Pellets
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.22g/cm³ASTM D792
MechanicalNominal ValueUnitTest Method
Tensile Strength (23°C)103MPaASTM D638
Tensile Elongation (Break, 23°C)2.0%ASTM D638
Flexural Modulus (23°C)4830MPaASTM D790
Flexural Strength (23°C)172MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C)64J/mASTM D256
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)243°CASTM D648
Melting Temperature 254°C
FlammabilityNominal ValueTest Method
Flame Rating HBUL 94
Resin Grade Manufacturer Category Trademark
TAROLOX GFR Taro Plast S.p.A. PBT TAROLOX
Texalan® 3 Series 385A Austin Novel Materials Co. Ltd. TPU-Polyester Texalan® 3 Series
VITAMIDE® AS30BK8522 Jackdaw Polymers Nylon 66 VITAMIDE®
Formolene® 6730J Formosa Plastics Corporation, U.S.A. PP Copolymer Formolene®
Sylvin 83037-80 Natural Sylvin Technologies Incorporated PVC, Unspecified Sylvin