OmniLon™ PA6/6 MS2

Category: Nylon 66 , Polyamide 66
Manufacturer: OMNI Plastics, LLC
Trademark: OmniLon™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: U8wqy6_OmniLon-PA6-6-MS2.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
High Lubricity, Wear Resistant, Nylon 6/6
General Information
Additive
  • Lubricant (2 ppm)
Features
  • Good wear resistance
  • Lubrication
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.15g/cm³ASTM D792
MechanicalNominal ValueUnitTest Method
Tensile Strength (Yield, 23°C)82.7MPaASTM D638
Tensile Elongation (Break)20%ASTM D638
Flexural Modulus 2900MPaASTM D790
Flexural Strength 121MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C, 3.18 mm)48J/mASTM D256
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (0.45 MPa, Unannealed, 3.18 mm)257°CASTM D648
FlammabilityNominal ValueTest Method
Flame Rating (3.18 mm)HBInternal method
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 2.0 - 4.0hr
Suggested Max Moisture 0.20%
Rear Temperature 260 - 293°C
Middle Temperature 271 - 293°C
Front Temperature 271 - 293°C
Nozzle Temperature 271 - 293°C
Processing (Melt) Temp 271 - 293°C
Mold Temperature 26.7 - 60.0°C
Back Pressure 0.345MPa
Resin Grade Manufacturer Category Trademark
Niblan F30 AE/V0 Soredi S.p.a. PBT Niblan
Armlen® PP School 20.1 Poly Plastic PP, Unspecified Armlen®
Dryflex® 662700S ELASTO SEBS Dryflex®
MAJORIS DW374 - 8229 AD majoris PP Copolymer MAJORIS
POLYfill PP CIP1001F Polykemi AB PP, Unspecified POLYfill