Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | Shanghai Utomer Material Science Co., Ltd. |
Trademark: | Utomer |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Tf8CTa_Utomer-UT370.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Utomer TPU which include ester and ether type. It's suitable for calendering and extrusion, which are used for shoes and clothing leatherette and compounding with PVC. |
General Information | |
---|---|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 68 to 72 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion Loss | 50.0 | mm³ | DIN 53516 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% Strain | 4.00 | MPa | |
300% Strain | 7.00 | MPa | |
Tensile Strength | 30.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 800 | % | ASTM D412 |
Tear Strength | 0.0800 | kN/m | ASTM D624 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | -20.0 | °C | ASTM D3418 |
Melting Temperature | 120 to 140 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Vital-Line SHM5505 | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | Vital-Line |
Comco POM C | Comco-Plastic GmbH | Acetal (POM) Copolymer | Comco |
LEXAN™ LUX2614 resin | SABIC Innovative Plastics Asia Pacific | PC | LEXAN™ |
Latilub 66-10T K/10 | LATI S.p.A. | Nylon 66 | Latilub |
Mafill® CR XM 6144 | Ravago Group | PP Copolymer | Mafill® |