RTP 807

Category: Acetal (POM) Copolymer , Acetal (POM) Copolymer
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: TO5FME_RTP-807.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Glass Fiber
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 40% filler by weight
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.70g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.20 - 0.30%ASTM D955
Moisture Content 0.15%
Additional InformationNominal ValueUnit
Primary Additive 40%
MechanicalNominal ValueUnitTest Method
Tensile Modulus 12800MPaASTM D638
Tensile Strength 117MPaASTM D638
Tensile Elongation (Yield)1.4 - 2.2%ASTM D638
Flexural Modulus 11000MPaASTM D790
Flexural Strength 172MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)75J/mASTM D256
Unnotched Izod Impact (3.20 mm)530J/mASTM D4812
FlammabilityNominal ValueTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 121°C
Drying Time 2.0hr
Dew Point -31.7°C
Processing (Melt) Temp 182 - 218°C
Mold Temperature 79.4 - 107°C
Injection Pressure 68.9 - 103MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
Viton® C-10 DuPont Performance Elastomers Fluorelastomer Viton®
Chemlon® 240GH Teknor Apex Company (Chem Polymer) Nylon 6 Chemlon®