| Category: | EVA , Ethylene Vinyl Acetate Copolymer |
| Manufacturer: | Southern Polymer, Inc. |
| Trademark: | PRIMALENE |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | TDuQ9R_PRIMALENE-WPP514E18.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
A 2.0 melt index vinyl acetate polyethylene Applications:
Features:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.935 | g/cm³ | |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 2.0 | g/10 min | ASTM D1238 |
| Vinyl Acetate Content | 18.2 | wt% |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 36 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | ASTM D638 | ||
| Yield | 5.24 | MPa | |
| Break | 11.4 | MPa | |
| Tensile Elongation | ASTM D638 | ||
| Yield | 260 | % | |
| Break | > 800 | % | |
| Flexural Modulus - 1% Secant | 60.3 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Instrumented Dart Impact (23°C) | 17.6 | J | ASTM D3763 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 63.9 | °C | ASTM D1525 |
| Peak Melting Temperature | 87.2 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 200 A SI 2 | RTP Company | Nylon 6 | RTP |
| Restramid PA 6 GWT 960 HF | Polimarky Spolka Jawna | Nylon 6 | Restramid |
| SLOVAMID® 66/6 GF 30 TS | Plastcom | Nylon 66/6 | SLOVAMID® 66/6 |
| NuSil MED-4780 | NuSil Technology | Rubber | NuSil |
| Cri-Line FDA-618-BR | Cri-Tech, Inc. | Fluorelastomer | Cri-Line |