Sarlink K-156 is suitable for exterior automotive applications and exhibits superior low temperature performance. |
General Information | |
---|---|
Features |
|
Appearance |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.940 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/5.0 kg) | 70 | g/10 min | ISO 1133 |
Molding Shrinkage (2.00 mm) | 1.1 to 1.6 | % | ISO 294-4 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D, 5 sec, Injection Molded) | 38 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Flexural Modulus | ISO 178 | ||
-40°C | 1070 | MPa | |
23°C | 265 | MPa |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress - Across Flow (100% Strain) | 7.90 | MPa | ISO 37 |
Tensile Stress - Across Flow (Break) | 10.2 | MPa | ISO 37 |
Tensile Elongation - Across Flow (Break) | 570 | % | ISO 37 |
Compression Set (70°C, 22 hr) | 74 | % | ISO 815 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength (-35°C) | No Break | ISO 180/A |
Additional Information | Nominal Value | Unit | Test Method |
---|---|---|---|
Apparent Shear Viscosity - 206 1/s, Capillary (200°C) | 198 | Pa·s | ISO 11443 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TULAMID® PA-SV30-L1 | UCC Shchekinoazot | Nylon 6 | TULAMID® |
ALCUDIA® EBA PA-1715 | REPSOL | EBA | ALCUDIA® EBA |
APEX® RM 8201 | Teknor Apex Company | PVC, Rigid | APEX® |
Osterlene® HE-3.5-3-stg | Osterman & Company | PS (HIPS) | Osterlene® |
Plaslube® PEEK T/GL20 | Techmer Engineered Solutions | PEEK | Plaslube® |