| Category: | PUR, Unspecified , Polyurethane |
| Manufacturer: | Crosspolimeri S.p.A. |
| Trademark: | TANEGUM |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Su3E6T_TANEGUM-ME-85-U2-SA.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
TANEGUM ME/85 U2 SA is a modified polyurethane technopolymer presenting many of the positive features of pure polyurethane and improved capabilities of extrudibility. TANEGUM ME/85 U2 SA also has good resistance properties to flex-fatigue and to abrasion. They are also suitable for electrical applications with resistance to ozone, hydrocarbons, oils, fats, fuels, and greases. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.30 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 86 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield) | 30.0 | MPa | IEC 60811 |
| Tensile Strain (Break) | 480 | % | IEC 60811 |
| Aging | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Change in Tensile Strength in Air (100°C, 168 hr) | 10 | % | IEC 60811 |
| Change in Tensile Strain at Break in Air (100°C, 168 hr) | -3.0 | % | IEC 60811 |
| Change in Tensile Stress (70°C, 4 hr, in SAE 20 Oil) | -15 | % | IEC 60811 |
| Change in Tensile Strain at Break (70°C, 4 hr, in SAE 20 Oil) | 32 | % | IEC 60811 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Hot Pressure Test - Penetration 1(80°C) | 16 | % | IEC 60811 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index | 23 | % | ASTM D2863 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 160 | °C | |
| Cylinder Zone 2 Temp. | 165 | °C | |
| Cylinder Zone 3 Temp. | 170 | °C | |
| Cylinder Zone 4 Temp. | 180 | °C | |
| Cylinder Zone 5 Temp. | 170 to 175 | °C | |
| Die Temperature | 175 to 185 | °C |
| Note Message | |
|---|---|
| 1 . | 4 hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| MIRASON™ 252 | Mitsui Chemicals, Inc. | LDPE | MIRASON™ |
| Caltex PP MT13 | GS Caltex | PP, Unspecified | Caltex PP |
| Kynar Superflex® 2501-20 | Arkema | PVDF | Kynar Superflex® |
| Jam PE 524H1 | Jam Petrochemical Company | HDPE, HMW | Jam PE |
| Petrotene® PP A3 G15 NTLA010 PH307 | Petropol Industry and Trade of Polymers LTDA | PP, Unspecified | Petrotene® PP |