Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Polykemi AB |
Trademark: | SCANAMID 6 |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | SkVndD_SCANAMID-6-B13-F30.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Glass fibre-reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.36 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 0.90 | -- | % | |
Flow | 0.30 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Stress | 170 | 125 | MPa | ISO 527-2 |
Tensile Strain (Break) | 3.0 | 5.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 8800 | 5600 | MPa | ISO 178 |
Flexural Stress | 240 | 150 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | |||
-20°C | -- | 8.0 | kJ/m² | |
23°C | 10 | 14 | kJ/m² |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature 1 | ||||
0.45 MPa, Unannealed | 215 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 205 | -- | °C | ISO 75-2/A |
Vicat Softening Temperature | > 200 | -- | °C | ISO 306/B50 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (1.60 mm) | HB | -- | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 650 | -- | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
NORYL™ LTA5020 resin | SABIC Innovative Plastics | PPE+PS | NORYL™ |
Globalene® PF0105 | Lee Chang Yung Chemical Industry Corp. | PP Alloy | Globalene® |
Jam PE 43X01 | Jam Petrochemical Company | HDPE | Jam PE |
Lupox® TE5000H | LG Chem Ltd. | PC+PBT | Lupox® |
Durethan® BKV 30 FN00 000000 | LANXESS Corporation | Nylon 6 | Durethan® |