PPS, 65% Glass Fiber / Mineral Processing Method: Injection Molding |
General Information | |
---|---|
Filler / Reinforcement |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.94 | g/cm³ | ISO 1183 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (23°C) | 19000 | MPa | ISO 527-2 |
Tensile Stress (23°C) | 140 | MPa | ISO 527-2 |
Tensile Strain (Break, 23°C) | 1.0 - 3.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 6.0 | kJ/m² | ISO 179 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 270 | °C | ISO 75-2/A |
Melting Temperature (DSC) | 280 | °C | ISO 3146 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | > 1.0E+14 | ohms·cm | ISO 3915 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | V-0 | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 130 - 150 | °C | |
Drying Time | 2.0 - 6.0 | hr | |
Processing (Melt) Temp | 310 - 340 | °C | |
Mold Temperature | 140 - 170 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Rilsan® AESN EP 076 TL | Arkema | Nylon 12 | Rilsan® |
TECHNYL STAR™ AFX 218 V60 BLACK 31N | Solvay Engineering Plastics | Nylon 66 | TECHNYL STAR™ |
Cri-Line LC-615-65 | Cri-Tech, Inc. | Fluorelastomer | Cri-Line |
Hyundai EP PPC HP908H | HYUNDAI EP Co., Ltd. | PP Copolymer | Hyundai EP PPC |
LNP™ THERMOCOMP™ DF004 compound | SABIC Innovative Plastics | PC | LNP™ THERMOCOMP™ |