Category: | Nylon 66/6 , Polyamide 66/6 Copolymer |
Manufacturer: | Polykemi AB |
Trademark: | SCANAMID 66.6 |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Rg1Ku6_SCANAMID-66-6-C12-F30.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Glass fibre reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.36 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.1 | % | |
Flow | 0.30 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 175 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 5.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 8800 | MPa | ISO 178 |
Flexural Stress | 243 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 6.0 | kJ/m² | |
23°C | 8.0 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179 | ||
-20°C | 40 | kJ/m² | |
23°C | 42 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 250 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 240 | °C | ISO 75-2/A |
Vicat Softening Temperature | > 230 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | HB | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 650 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SEETEC LLDPE UL314P | Lotte Chemical Corporation | LLDPE | SEETEC LLDPE |
Asaprene™ T-437 | AKelastomers | SBS | Asaprene™ |
HAIPLEN H50 C10 | Taro Plast S.p.A. | PP Homopolymer | HAIPLEN |
IROSTIC® S 8612 | Huntsman Corporation | TPU, Unspecified | IROSTIC® |
LNP™ COLORCOMP™ E1000 compound | SABIC Innovative Plastics Europe | PEI | LNP™ COLORCOMP™ |