Category: | PP, Unspecified , Polypropylene |
Manufacturer: | SAMBARK |
Trademark: | SUPRAN® LFT PP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Qkf9Yk_SUPRAN-LFT-PP-1335F.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
35% long glass fiber reinforced non flammability purpose Polypropylene. |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.29 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 0.20 | % | ASTM D648 |
Water Absorption (24 hr) | 0.020 | % | ASTM D570 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 104 | MPa | ASTM D638 |
Tensile Elongation (Break) | 2.7 | % | ASTM D638 |
Flexural Modulus | 7600 | MPa | ASTM D790 |
Flexural Strength | 163 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact | ASTM D256 | ||
-30°C | 210 | J/m | |
23°C | 210 | J/m |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 156 | °C | ASTM D648 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating | V-0 | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 90.0 | °C | |
Drying Time | 2.0 | hr | |
Processing (Melt) Temp | 210 to 220 | °C | |
Mold Temperature | 40.0 to 70.0 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
tefabloc® TP SD 300 50A | Mitsubishi Chemical Performance Polymers, Inc. | TPE | tefabloc® |
Catalyst CT/1 | Solvay Specialty Polymers | Polyolefin, Unspecified | Catalyst |
Evoprene™ G 3291 | AlphaGary | SEBS | Evoprene™ G |
Halar® 6614 | Solvay Specialty Polymers | ECTFE | Halar® |
Hylex® P1325G20FRMA | Ravago Manufacturing Americas, LLC | PC | Hylex® |