Category: | PP Copolymer , Polypropylene Copolymer |
Manufacturer: | Ferro Corporation |
Trademark: | RxLOY™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | PnxA3I_RxLOY-NPP00NP03NA.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
RxLOY™ NPP00NP03NA is a Polypropylene Copolymer (PP Copolymer) material. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. |
General Information | |
---|---|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.908 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 2.5 | g/10 min | ASTM D1238 |
Molding Shrinkage | ASTM D955 | ||
Flow | 1.0 | % | |
Across Flow | 2.2 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield, 23°C) | 11.7 | MPa | ASTM D638 |
Tensile Elongation (Break, 23°C) | 400 | % | ASTM D638 |
Flexural Modulus | ASTM D790 | ||
1% Secant : 23°C | 124 | MPa | |
Tangent : 23°C | 172 | MPa | |
Flexural Strength (Yield, 23°C) | 9.65 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | No Break | ASTM D256 | |
Unnotched Izod Impact (23°C) | No Break | ASTM D256 | |
Gardner Impact | > 36.2 | J | ASTM D5420 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 140 | °C | ASTM D1525 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Royalene® 580HT | Lion Copolymer, LLC | EPDM | Royalene® |
THERMORUN® QT99ZA | Mitsubishi Chemical Corporation | TPO (POE) | THERMORUN® |
Unichem 8092 | Colorite Polymers | PVC, Unspecified | Unichem |
ELASTOSIL® LR 3040/70 A/B | Wacker Chemie AG | Silicone | ELASTOSIL® LR |
TechnoGreen PP LGF 60-10-04 | TechnoCompound GmbH | PP, Unspecified | TechnoGreen |