| Category: | PP, Unspecified , Polypropylene |
| Manufacturer: | KOPLA Co., Ltd. |
| Trademark: | KOPLA PP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Pmg0rs_KOPLA-PP-KPG1010.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
KOPLA PP KPG1010 is a Polypropylene material filled with glass fiber. It is available in Asia Pacific. Primary attribute of KOPLA PP KPG1010: Flame Rated. Typical application of KOPLA PP KPG1010: Automotive |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.990 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (3.18 mm) | 0.40 to 0.60 | % | ASTM D955 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale) | 105 | ASTM D785 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield, 23°C) | 49.0 | MPa | ASTM D638 |
| Tensile Elongation (Break, 23°C) | 4.0 | % | ASTM D638 |
| Flexural Modulus (23°C) | 2260 | MPa | ASTM D790 |
| Flexural Strength (23°C) | 83.4 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact | 78 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (0.45 MPa, Unannealed) | 140 | °C | ASTM D648 |
| Melting Temperature | 163 | °C |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 1403 P | RTP Company | PPSU | RTP |
| Spartech Polycom PP5220 | Spartech Polycom | PP Homopolymer | Spartech |
| 4PROP® 5C14300 | 4Plas | PP Copolymer | 4PROP® |
| Kepamid® 1325GFS | Korea Engineering Plastics Co., Ltd | Nylon 6 | Kepamid® |
| Karina GRAY PVC COMPOUND 750-18/473-F-IS-BZ | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |