Lifoflex® UV FLAM 60700

Category: TPE , Thermoplastic Elastomer
Manufacturer: Müller Kunststoffe GmbH
Trademark: Lifoflex®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: PPzxWY_LifoflexUVFLAM60700.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Lifoflex FLAM are a range of halogen-free flame retardant thermoplastic elastomers (TPEs) designed to meet the most demanding applications where resistance to ignition and burning are important features.

Lifoflex FLAM compounds contain additives to give them better resistance to burning compared to general TPE grades. The range includes halogen, chlorine and antimony free grades which are low smoke and compliant with the Restriction of Hazardous Substances (RoHS) directives, offering flame retardancy without the use of polybrominated diphenyl ether (PBDE).
General Information
Additive
  • Flame retardancy
Features
  • Chlorine Free
  • Low smoke
  • Good flexibility
  • Good adhesion
  • Halogen-free
  • No antimony
  • Flame retardancy
Uses
  • Wire and cable applications
  • Electronic insulation
  • Washer
  • Washer
  • Reflector
  • Connector
  • Profile
Agency Ratings
  • EU 2003/11/EC
RoHS Compliance
  • RoHS compliance
UL File Number
  • W249957
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 1.07g/cm³ISO 1183
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A, 3 sec)60DIN 53505
ElastomersNominal ValueUnitTest Method
Tensile Stress - Across Flow (Yield)3.60MPaDIN 53504
Tensile Elongation - Across Flow (Break)700%DIN 53504
Compression Set ISO 815
    23°C, 72 hr 16%ISO 815
    70°C, 22 hr 36%ISO 815
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.50 mm)V-0UL 94
Glow Wire Ignition Temperature (3.00 mm)850 650°CIEC 60695-2-13
Drip Formation 1ST2DIN 5510-2
Smoke Formation 2SR2DIN 5510-2
Flammability 3S3DIN 5510-2
InjectionNominal ValueUnit
Drying Temperature 80.0°C
Drying Time 2.0 - 3.0hr
Rear Temperature 170 - 180°C
Middle Temperature 180 - 190°C
Front Temperature 190 - 200°C
Nozzle Temperature 200 - 210°C
Mold Temperature 15.0 - 50.0°C
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 150 - 160°C
Cylinder Zone 2 Temp. 160 - 170°C
Cylinder Zone 3 Temp. 170 - 180°C
Cylinder Zone 4 Temp. 180 - 190°C
Die Temperature 180 - 200°C
Note Message
1 .500x10x6mm
2 .500x10x6mm
3 .500x10x6mm
Resin Grade Manufacturer Category Trademark
POLYPRO® SB9108 YUHWA Korea Petrochemical Ind. Co., Ltd. PP Copolymer POLYPRO®
Monprene® CP-19237 Teknor Apex Company TPE Monprene®
Cevian® SEHG30 PlastxWorld Inc. ABS Cevian®
Globalprene® 3520 Lee Chang Yung Chemical Industry Corp. SBS Globalprene®
IDI SMC S52 (Glass Content 22%) IDI Composites International TS, Unspecified IDI SMC