Moplen EP300N is a heterophasic copolymer for injection moulding. The product offers an excellent balance of stiffness, impact strength and processability. Typical applications of Moplen EP300N are packaging, housewares and automotive parts. Moplen EP300N is suitable for food contact. It is not intended for medical and pharmacuetical applications. |
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.900 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 15 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield) | 24.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 6.5 | % | ISO 527-2 |
Flexural Modulus - 1% Secant 1 | 1100 | MPa | ISO 178 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (0.45 MPa, Unannealed) | 75.0 | °C | ISO 75-2/B |
Vicat Softening Temperature | 146 | °C | ISO 306/A50 |
Accelerated Oven Ageing 2(150°C) | 360 | hr | ISO 4577 |
Note Message | |
---|---|
1 . | 25 mm/min |
2 . | Forced Circulation |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 203 FR XB | RTP Company | Nylon 66 | RTP |
YUPLENE® B330F | SK Global Chemical | PP Impact Copolymer | YUPLENE® |
Aegis® BarrierPro2™ | Honeywell | HPPA | Aegis® |
Durez® 33771 | Sumitomo Bakelite North America, Inc. | Phenolic | Durez® |
Karina BLACK PVC COMPOUND 75930-48/ 1-F-AC-LF | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |