Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Teknor Apex Company |
Trademark: | Monprene® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | OwS0Hy_Monprene-OM-12250-01.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Monprene®OM-12250-01 is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Monprene®The main characteristics of the OM-12250-01 are: strong adhesion. Typical application areas include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.968 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 1.5 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shore A, 1 second, injection molding | 53 | ASTM D2240 | |
Shore A, 5 seconds, injection molding | 50 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (300% Strain) | 3.10 | MPa | ASTM D412 |
Tensile Strength (Break) | 7.58 | MPa | ASTM D412 |
Tensile Elongation (Break) | 500 | % | ASTM D412 |
Additional Information | Nominal Value | ||
---|---|---|---|
Adhesion to ABS | |||
Adhesion to PC | |||
Adhesion to PC/ABS |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 60.0 | °C | |
Drying Time | 2.0 - 4.0 | hr | |
Rear Temperature | 138 - 188 | °C | |
Middle Temperature | 154 - 199 | °C | |
Front Temperature | 154 - 216 | °C | |
Nozzle Temperature | 154 - 221 | °C | |
Processing (Melt) Temp | 166 - 221 | °C | |
Mold Temperature | 10.0 - 32.2 | °C | |
Injection Pressure | 1.38 - 5.52 | MPa | |
Back Pressure | 0.172 - 0.862 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
Moisture can degrade the material. Drying is suggested. This can be accomplished by placing the material in a desiccant dryer for 2 to 4 hours at 140°F. |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 138 - 149 | °C | |
Cylinder Zone 2 Temp. | 149 - 160 | °C | |
Cylinder Zone 3 Temp. | 160 - 182 | °C | |
Cylinder Zone 5 Temp. | 160 - 182 | °C | |
Die Temperature | 160 - 182 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Witcom PC/ABS AS-S | Witcom Engineering Plastics B.V. | PC+ABS | Witcom PC/ABS |
Unichem 7500 | Colorite Polymers | PVC, Unspecified | Unichem |
AMTOPP BA25 | Inteplast Group | PP, Unspecified | AMTOPP |
Cevian®-V T500, T500SF | Daicel Polymer Ltd. | ABS | Cevian®-V |
LEXAN™ 223R resin | SABIC Innovative Plastics | PC | LEXAN™ |