Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
Manufacturer: | COIM S.p.A. |
Trademark: | LARIPUR® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | OlXRs8_LARIPUR-LPR-7060.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
LARIPUR®LPR 7060 is a thermoplastic polyurethane elastomer (polyether)(TPU-polyether) material,. This product is available in North America, Latin America or Europe. The processing method is extrusion or injection molding. LARIPUR®The main features of LPR 7060 are:
Typical application areas include:
|
General Information | |
---|---|
Features |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.07 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 69 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
50% strain | 1.80 | MPa | ASTM D412 |
100% strain | 2.50 | MPa | ASTM D412 |
300% strain | 5.40 | MPa | ASTM D412 |
Tensile Strength (Break) | 39.1 | MPa | ASTM D412 |
Tensile Elongation (Break) | 730 | % | ASTM D412 |
Tear Strength | 55.0 | kN/m | ASTM D624 |
Compression Set | ASTM D395 | ||
23°C, 70 hr | 20 | % | ASTM D395 |
70°C, 22 hr | 44 | % | ASTM D395 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 66.0 | °C | ASTM D1525 |
Additional Information |
---|
Abrasion loss, DIN 53516: 30 mm³ |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SCHULAMID® 66 GBF 3020 | A. Schulman Europe | Nylon 66 | SCHULAMID® |
Akulon® F136-C1 | DSM Engineering Plastics | Nylon 6 | Akulon® |
Cheng Yu NG1300S | Cheng Yu Plastic Company Limited | Nylon 66 | Cheng Yu |
Dynaflex™ G7930-9001-02 | PolyOne Corporation | TPE | Dynaflex™ |
KYOCERA KE-G240V | KYOCERA Chemical Corporation | Epoxy | KYOCERA |