| Category: | Acetal (POM) Copolymer , Acetal (POM) Copolymer |
| Manufacturer: | BARLOG plastics GmbH |
| Trademark: | KEBAFORM® C |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | OgvKRZ_KEBAFORM-C-901-CB.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| POM Copolymer unreinforced, electr. conductive |
| General Information | |
|---|---|
| Features |
|
| Resin ID (ISO 1043) |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.39 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 7.0 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2700 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 55.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 5.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 4.5 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength (23°C) | No Break | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 110 | °C | ISO 75-2/A |
| Melting Temperature 1 | 166 | °C | ISO 11357-3 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 2.0E+3 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+7 | ohms·cm | IEC 60093 |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| tefabloc® TO 228 | Mitsubishi Chemical Performance Polymers, Inc. | SEBS | tefabloc® |
| SLOVAMID® 66/6 GF 30 TS | Plastcom | Nylon 66/6 | SLOVAMID® 66/6 |
| TOTAL Polypropylene Lumicene® MR 30MC2 | TOTAL Refining & Chemicals | PP Random Copolymer | TOTAL Polypropylene |
| Fainplast PVC RE 140/1 | Fainplast Compounds S.r.l | PVC, Rigid | Fainplast PVC |
| Hytrel® HTR8223 BK320 | DuPont Performance Polymers | TPC-ET | Hytrel® |