Category: | PP, Unspecified , Polypropylene |
Manufacturer: | RTP Company |
Trademark: | RTP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | NsNm1s_RTP199X123298B.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
ESD Protection - Permanently Static Dissipative - Impact Modified - UV Stabilized |
General Information | |
---|---|
Additive |
|
Features |
|
RoHS Compliance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.920 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.20 mm) | 0.10 - 0.20 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 483 | MPa | ASTM D638 |
Tensile Strength | 11.0 | MPa | ASTM D638 |
Tensile Elongation (Yield) | > 10 | % | ASTM D638 |
Flexural Modulus | 552 | MPa | ASTM D790 |
Flexural Strength | 15.9 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.20 mm) | 750 | J/m | ASTM D256 |
Unnotched Izod Impact (3.20 mm) | No Break | ASTM D4812 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Surface Resistivity | < 1.0E+9 | ohms | ESD STM11.11 |
Static Decay | sec | FTMS 101C 4046.1 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79 | °C | |
Drying Time | 2.0 | hr | |
Processing (Melt) Temp | 191 - 232 | °C | |
Mold Temperature | 32 - 66 | °C | |
Injection Pressure | 68.9 - 103 | MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Pyramid™ PEEK KD2250 | Polymics, Ltd. | PEEK | Pyramid™ PEEK |
NEXUS PE LLDPE-B118 | Nexus Resin Group, LLC. | LLDPE | NEXUS PE |
Badamid® LC70 FR HF | Bada AG | Nylon 6+Nylon 66/6 | Badamid® |
Karina WHITE COLOR CONCENTRATE MBU 10/ 70-IE | Karina Ind. e Com. de Plásticos Ltda | EVA | Karina |
XYLEX™ X8409AC resin | SABIC Innovative Plastics | PC+Polyester | XYLEX™ |