Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Teknor Apex Company |
Trademark: | Sarlink® TPE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Ng8IDE_Sarlink-TPE-ME-2555B-XRD.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Sarlink ME-2500 Series are high-flow injection molding materials with excellent UV resistance and adhesion to glass. |
General Information | |
---|---|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.11 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 4.0 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ISO 868 | ||
Shaw A, 1 sec | 55 | ISO 868 | |
Shaw A, 5 seconds | 52 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ISO 37 | ||
Transverse flow : 100% strain, 23°C | 1.30 | MPa | ISO 37 |
Flow : 100% strain, 23°C | 1.40 | MPa | ISO 37 |
Tensile Strength | |||
Transverse flow : fracture, 23°C | 6.20 | MPa | ISO 37 |
Flow : fracture, 23°C | 5.80 | MPa | ASTM D412 |
Tensile Elongation | |||
Transverse flow : fracture, 23°C | 830 | % | ISO 37 |
Flow : fracture, 23°C | 820 | % | ASTM D412 |
Compression Set (70°C, 22 hr) | 30 | % | ISO 815 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air | ISO 188 | ||
110°C, 1008 hr | 9.0 | % | ISO 188 |
125°C, 1008 hr | -12 | % | ISO 188 |
Additional Information | Nominal Value | Unit | |
---|---|---|---|
Apparent Shear Viscosity - @ 206 1/sec (200°C) | 130 | Pa·s |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 170 - 190 | °C | |
Middle Temperature | 175 - 195 | °C | |
Front Temperature | 180 - 205 | °C | |
Nozzle Temperature | 180 - 205 | °C | |
Processing (Melt) Temp | 180 - 205 | °C | |
Mold Temperature | 15.0 - 40.0 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 0.172 - 0.862 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 176°F (80°C). |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP EMI 360.6 FR | RTP Company | PC | RTP |
Spartech Polycom PP7150 | Spartech Polycom | PP Copolymer | Spartech |
NILENE® E15 K15TE | Taro Plast S.p.A. | PP Copolymer | NILENE® |
DINALON® PA 6.6 | Grupo Repol | Nylon 66 | DINALON® |
ExxonMobil™ LDPE LD 331.08 | ExxonMobil Chemical | LDPE | ExxonMobil™ LDPE |