Crastin® LW9030 BK851

Category: PBT , THERMOPLASTIC POLYESTER RESIN
Manufacturer: DuPont Performance Polymers
Trademark: Crastin®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: NTvUSa_Crastin-LW9030-BK851.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics
General Information
Filler / Reinforcement
  • Glass Fiber, 30% Filler by Weight
Agency Ratings
  • UL Unspecified Rating
Processing Method
  • Injection Molding
Part Marking Code (ISO 11469)
  • >PBT+ASA-GF30<
Resin ID (ISO 1043)
  • PBT+ASA-GF30
PhysicalNominal ValueUnitTest Method
Density 1.44g/cm³ISO 1183
MechanicalNominal ValueUnitTest Method
Tensile Modulus 9200MPaISO 527-2
Tensile Stress (Break)125MPaISO 527-2
Tensile Strain (Break)2.0%ISO 527-2
Flexural Modulus 8500MPaISO 178
Flexural Stress 180MPaISO 178
ImpactNominal ValueUnitTest Method
Charpy Notched Impact Strength ISO 179/1eA
    -30°C 7.0kJ/m²
    23°C 9.0kJ/m²
Charpy Unnotched Impact Strength ISO 179/1eU
    -30°C 45kJ/m²
    23°C 50kJ/m²
Notched Izod Impact Strength ISO 180/1A
    -30°C 7.0kJ/m²
    23°C 7.0kJ/m²
Unnotched Izod Impact Strength ISO 180/1U
    -30°C 50kJ/m²
    23°C 45kJ/m²
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature
    0.45 MPa, Unannealed 210°CISO 75-2/B
    1.8 MPa, Unannealed 170°CISO 75-2/A
Melting Temperature 1225°CISO 11357-3
FlammabilityNominal ValueUnitTest Method
Flammability Classification (1.50 mm)HBIEC 60695-11-10, -20
Oxygen Index 20%ISO 4589-2
Note Message
1 .10°C/min
Resin Grade Manufacturer Category Trademark
Sylvin 9604-85C Black Sylvin Technologies Incorporated PVC, Unspecified Sylvin
Hangzhou Plastic PS/PVDC/PE Hangzhou Plastic Industry Co., Ltd. Film, PS/PVDC/PE Hangzhou Plastic
HAIPLEN EP50 T4 X0 Taro Plast S.p.A. PP Copolymer HAIPLEN
ESTADIENE 0417 GF Cossa Polimeri S.r.l. ABS ESTADIENE
Kumho KHS 68 Korea Kumho Petrochemical Co., Ltd. SBR, Emulsion Kumho KHS