Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Elastocon TPE Technologies |
Trademark: | Elastocon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | NTOXTv_Elastocon-CLR65.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface finish. Elastocon?? CLR65 is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon?? CLR65 can be overmolded onto polypropylene. Elastocon® CLR65 is supplied as ready to use pellets in 1000 lb. quantities. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.890 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 62 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 2.20 | MPa | ASTM D412 |
Tensile Strength (Yield) | 8.60 | MPa | ASTM D412 |
Tensile Elongation (Break) | 630 | % | ASTM D412 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 166 - 177 | °C | |
Front Temperature | 182 - 188 | °C | |
Nozzle Temperature | 193 - 204 | °C | |
Mold Temperature | 21.1 - 37.8 | °C | |
Injection Rate | Fast | ||
Back Pressure | 0.689 - 1.38 | MPa |
Injection instructions |
---|
Elastocon® CLR40 thermoplastic elastomer compound does not require drying. |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Hopper Temperature | < 79.4 | °C | |
Cylinder Zone 1 Temp. | 149 - 177 | °C | |
Cylinder Zone 2 Temp. | 149 - 177 | °C | |
Cylinder Zone 3 Temp. | 149 - 177 | °C | |
Cylinder Zone 4 Temp. | 149 - 177 | °C | |
Cylinder Zone 5 Temp. | 149 - 177 | °C | |
Die Temperature | 149 - 177 | °C |
Extrusion instructions |
---|
Compression ratio: 2.5 to 3.0 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
REPOL® MI3535 | Reliance Industries Limited | PP Impact Copolymer | REPOL® |
WONDERLITE® PC-175 | CHI MEI CORPORATION | PC | WONDERLITE® |
APEX® 3710-85NT1 | Teknor Apex Company | PVC, Flexible | APEX® |
apilon 52c® C S200 | API SpA | TPU-Polyester | apilon 52c® |
Elastollan® 1190 A 10 FHF 000 | BASF Polyurethanes GmbH | TPU-Polyether | Elastollan® |