Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | API SpA |
Trademark: | apilon 52® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | NItQK3_apilon-52-D-30-L.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
apilon 52®D 30 L is a thermoplastic polyurethane elastomer (polyester)(TPU-polyester) product,. It can be processed by injection molding and is available in Europe. apilon 52®The application areas of D 30 L include engineering/industrial accessories, electrical/electronic applications, electrical appliances, tools and home applications. Features include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A, 15 seconds | 87 | ASTM D2240 | |
Shaw D, 3 seconds | 40 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | ASTM D638 | ||
-- | 45.0 | MPa | ASTM D638 |
100% strain | 6.00 | MPa | ASTM D638 |
300% strain | 12.0 | MPa | ASTM D638 |
Tensile Elongation (Break) | 550 | % | ASTM D638 |
Abrasion Resistance | 30.0 | mm³ | DIN 53516 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength 1 | 100 | kN/m | ASTM D624 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (-20°C) | No Break | ASTM D256 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 110 | °C | |
Drying Time | 2.0 | hr | |
Suggested Max Moisture | 0.070 | % | |
Rear Temperature | 180 - 190 | °C | |
Middle Temperature | 185 - 200 | °C | |
Front Temperature | 190 - 215 | °C | |
Nozzle Temperature | 200 - 230 | °C | |
Mold Temperature | 30.0 - 60.0 | °C | |
Injection Pressure | 50.0 - 100 | MPa | |
Injection Rate | Slow-Moderate |
Injection instructions |
---|
Back Pressure: Medium to LowLocking Pressure: High |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 110 | °C | |
Drying Time | 2.0 | hr | |
Suggested Max Moisture | 0.070 | % | |
Cylinder Zone 1 Temp. | 160 - 185 | °C | |
Cylinder Zone 2 Temp. | 170 - 200 | °C | |
Cylinder Zone 3 Temp. | 175 - 210 | °C | |
Cylinder Zone 4 Temp. | 180 - 220 | °C | |
Die Temperature | 170 - 210 | °C |
Extrusion instructions |
---|
L/D Ratio: 20:1 to 30:1Compression Ratio: 1:2.5 to 1:3 |
Note Message | |
---|---|
1 . | Without Notch |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SPESIN® KP212G15V0W3 | Kolon Plastics, Inc. | PBT | SPESIN® |
DOW™ HDPE 82054T | The Dow Chemical Company | HDPE | DOW™ HDPE |
BONDYRAM® TL1306 | Polyram Ram-On Industries | PP, Unspecified | BONDYRAM® |
ECOGRAN® PSI BLK | Eurocompound Polymers | PS (GPPS) | ECOGRAN® |
OmniLon™ PA6/6 S12 FD | OMNI Plastics, LLC | Nylon 66 | OmniLon™ |