| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | Teknor Apex Company |
| Trademark: | Sarlink® TPE |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | NBTGQM_Sarlink-TPE-ME-2180N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Sarlink®TPE ME-2180N is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is injection molding. Sarlink®The typical application field of TPE ME-2180N is: automobile industry |
| General Information | |
|---|---|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.18 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 3.0 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 80 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain | 2.76 | MPa | ASTM D412 |
| 300% strain | 3.52 | MPa | ASTM D412 |
| Tensile Strength (Break) | 8.62 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 700 | % | ASTM D412 |
| Tear Strength | 28.0 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 199 - 210 | °C | |
| Middle Temperature | 204 - 216 | °C | |
| Front Temperature | 210 - 221 | °C | |
| Nozzle Temperature | 216 - 227 | °C | |
| Processing (Melt) Temp | 216 - 227 | °C | |
| Mold Temperature | 35.0 - 65.6 | °C | |
| Injection Pressure | 1.38 - 6.89 | MPa | |
| Injection Rate | Fast | ||
| Back Pressure | 0.172 - 0.862 | MPa | |
| Screw Speed | 50 - 120 | rpm | |
| Cushion | 3.81 - 25.4 | mm |
| Injection instructions |
|---|
| 无需干燥。但如果湿度过大,则将粒料在150°F (65°C)的温度下干燥2-4小时。 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 193 - 204 | °C | |
| Cylinder Zone 2 Temp. | 199 - 210 | °C | |
| Cylinder Zone 3 Temp. | 204 - 216 | °C | |
| Cylinder Zone 5 Temp. | 210 - 221 | °C | |
| Die Temperature | 216 - 227 | °C |
| Extrusion instructions |
|---|
| 螺杆转速30 - 100 rpm |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 2800 B-75A FR | RTP Company | TPV | RTP |
| Andur 7501 DPLF/Curene® 442 | Anderson Development Company | PUR-Ether/TDI | Andur |
| ELASTOSIL® R 401/40 | Wacker Chemie AG | Silicone | ELASTOSIL® R |
| Hostalen ACP 5231 D | LyondellBasell Industries | HDPE | Hostalen |
| TECHNYL® A 21T3 V25 BLACK 15N | Solvay Engineering Plastics | Nylon 66 | TECHNYL® |