High viscosity flame-retardant and heat stabilized Polyamide 6 grade; halogen- and phosphorus-free |
General Information | |
---|---|
Features |
|
UL File Number |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.20 | -- | g/cm³ | ISO 1183/A |
Viscosity Number | 195 | -- | cm³/g | ISO 307 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 3200 | 1200 | MPa | ISO 527-2/1A/1 |
Tensile Stress (Yield) | 75.0 | 50.0 | MPa | ISO 527-2/1A/50 |
Tensile Strain (Yield) | 4.0 | > 50 | % | ISO 527-2/1A/50 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 4.0 | -- | kJ/m² | ISO 179/1eA |
23°C | 5.0 | 12 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | No Break | -- | ISO 179/1eU | |
23°C | No Break | No Break | ISO 179/1eU |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, not annealed | 197 | -- | °C | ISO 75-2/Bf |
1.8 MPa, not annealed | 68.0 | -- | °C | ISO 75-2/Af |
Vicat Softening Temperature | ||||
-- | 216 | -- | °C | ISO 306/A50 |
-- | 200 | -- | °C | ISO 306/B50 |
Ball Pressure Test (200°C) | Pass | -- | IEC 60695-10-2 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Comparative Tracking Index | 600 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Rate | ISO 3795 | |||
0.750mm, automatic fire extinguishing | 0.0 | -- | mm/min | ISO 3795 |
1.50mm, automatic fire extinguishing | 0.0 | -- | mm/min | ISO 3795 |
3.00mm, automatic fire extinguishing | 0.0 | -- | mm/min | ISO 3795 |
Flammability Classification | IEC 60695-11-10, -20 | |||
0.750 mm | V-0 | -- | IEC 60695-11-10, -20 | |
1.50 mm | V-0 | -- | IEC 60695-11-10, -20 | |
3.00 mm | V-0 | -- | IEC 60695-11-10, -20 | |
Glow Wire Flammability Index | IEC 60695-2-12 | |||
0.750 mm | 960 | -- | °C | IEC 60695-2-12 |
1.50 mm | 960 | -- | °C | IEC 60695-2-12 |
3.00 mm | 960 | -- | °C | IEC 60695-2-12 |
Glow Wire Ignition Temperature | IEC 60695-2-13 | |||
0.750 mm | 725 | -- | °C | IEC 60695-2-13 |
1.50 mm | 725 | -- | °C | IEC 60695-2-13 |
3.00 mm | 725 | -- | °C | IEC 60695-2-13 |
Oxygen Index | 34 | -- | % | ISO 4589-2 |
Additional Information |
---|
干燥 1.) Not for use in food contact applications2.) Not for use in medical or pharmaceutical applications |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 3.0 - 4.0 | hr | |
Suggested Max Moisture | 0.040 - 0.10 | % | |
Hopper Temperature | 70.0 | °C | |
Rear Temperature | 230 | °C | |
Middle Temperature | 245 | °C | |
Front Temperature | 260 | °C | |
Processing (Melt) Temp | < 260 | °C | |
Mold Temperature | 60.0 - 100 | °C | |
Injection Pressure | 80.0 - 140 | MPa | |
Injection Rate | Moderate | ||
Holding Pressure | 40.0 - 85.0 | MPa | |
Back Pressure | 2.00 - 8.00 | MPa | |
Screw Speed | 250 | mm/sec |
Injection instructions |
---|
During transport one component of the dryblend can go more to the bottom. It is therefore recommended to tumble the material before use to assure an even distribution of the dryblend components. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Makroblend® EL703 | Covestro - Polycarbonates | PC+PET | Makroblend® |
Maxelast® S4740 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
Cheng Yu C6600 | Cheng Yu Plastic Company Limited | PC+ABS | Cheng Yu |
Hytrel® 5526 | DuPont Performance Polymers | TPC-ET | Hytrel® |
O'Tech OW 645 | O'Tech Corporation | PVC, Unspecified | O'Tech |