Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | DESCO Co., Ltd. |
Trademark: | DESLON™ 6 |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | MXkRuN_DESLON-6-DSC102WG6.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Descriptions: DESLON™ DSC102WG6 is one of the brands which made by Polyamide6 that filled Glass Fiber 30% and good weatherability goods. It provides good mechanical property, fluidity property and injection molding property. Applications: DESLON™ DSC102WG6 is one of the most-used for high strength, weatherability goods,. such as electric and electronic of goods and Coil Bobbin, Lamp Housing, etc. |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.35 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 0.40 - 0.70 | % | |
Water Absorption (23°C, 24 hr) | 1.3 | % | ASTM D570 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 121 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 157 | MPa | ASTM D638 |
Tensile Elongation (Break) | 3.0 | % | ASTM D638 |
Flexural Modulus | 7350 | MPa | ASTM D790 |
Flexural Strength | 216 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact | 98 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 220 | °C | ASTM D648 |
1.8 MPa, not annealed | 210 | °C | ASTM D648 |
Melting Temperature | 220 | °C | DSC |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 2.0E+12 | ohms·cm | ASTM D257 |
Dielectric Strength | 20 | kV/mm | ASTM D149 |
Dielectric Constant (1 MHz) | 4.00 | ASTM D150 | |
Arc Resistance | 160 | sec | ASTM D495 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 120 | °C | |
Drying Time | 3.0 - 5.0 | hr | |
Suggested Max Moisture | < 0.20 | % | |
Rear Temperature | 240 - 250 | °C | |
Middle Temperature | 250 - 260 | °C | |
Front Temperature | 250 - 270 | °C | |
Nozzle Temperature | 255 - 270 | °C | |
Processing (Melt) Temp | 255 - 270 | °C | |
Mold Temperature | 80.0 - 100 | °C |
Injection instructions |
---|
Speed: 30 to 60%Pressure 1st: 30 to 70%Pressure 2nd: 30 to 70Holding Pressure: 10 to 30% |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Radilon® A RV200L 100 NAT | Radici Plastics | Nylon 66 | Radilon® |
Tecomid® NB40 NL RM | Eurotec Engineering Plastics | Nylon 6 | Tecomid® |
Badamid® LA70 GF25 H | Bada AG | Nylon 66 | Badamid® |
Alpha PVC 2228GBF-75S CLEAR 000X | AlphaGary | PVC, Flexible | Alpha PVC |
InnoTuf® HP-2170D | Innovative Polymers, Inc. | TSU | InnoTuf® |