Ultramid® B3S BK00464 is a Polyamide 6 (Nylon 6) product. It can be processed by injection molding and is available in North America. Typical application: Automotive.

Characteristics include:
  • REACH Compliant
  • RoHS Compliant
  • Chemical Resistant
General Information
Features
  • Oil Resistant
Agency Ratings
  • EC 1907/2006 (REACH)
RoHS Compliance
  • RoHS Compliant
Appearance
  • Black
Forms
  • Pellets
Processing Method
  • Injection Molding
Multi-Point Data
  • Creep Modulus vs. Time (ISO 11403-1)
  • Isochronous Stress vs. Strain (ISO 11403-1)
  • Isothermal Stress vs. Strain (ISO 11403-1)
  • Secant Modulus vs. Strain (ISO 11403-1)
  • Shear Modulus vs. Temperature (ISO 11403-1)
  • Specific Volume vs Temperature (ISO 11403-2)
  • Viscosity vs. Shear Rate (ISO 11403-2)
PhysicalDryConditionedUnitTest Method
Density 1.13--g/cm³ISO 1183
Melt Volume-Flow Rate (MVR) (275°C/5.0 kg)175--cm³/10minISO 1133
Water Absorption ISO 62
     Saturation, 23°C 9.5--%
     Equilibrium, 23°C, 50% RH 3.0--%
MechanicalDryConditionedUnitTest Method
Tensile Modulus (23°C)34001200MPaISO 527-2
Tensile Stress (Yield, 23°C)88.045.0MPaISO 527-2
Tensile Strain (Yield, 23°C)3.820%ISO 527-2
Nominal Tensile Strain at Break (23°C)10> 50%ISO 527-2
Flexural Modulus (23°C)2900--MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength ISO 179
     -30°C 3.0--kJ/m²
     23°C 4.050kJ/m²
Charpy Unnotched Impact Strength ISO 179
     -30°C 200--kJ/m²
     23°C 250 kJ/m²No Break
Notched Izod Impact Strength (23°C)3.0--kJ/m²ISO 180
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)65.0--°CISO 75-2/A
Melting Temperature (DSC) 220--°CISO 3146
InjectionDryUnit
Drying Temperature 80.0°C
Drying Time 2.0 to 4.0hr
Suggested Max Moisture 0.15%
Processing (Melt) Temp 240 to 285°C
Mold Temperature 65.0 to 80.0°C
Injection Pressure 3.50 to 12.5MPa
Injection Rate Fast
Resin Grade Manufacturer Category Trademark
Raditer® B RV200 Radici Plastics PBT Raditer®
Safron® R101-01NU Safripol (PTY) LTD PP Random Copolymer Safron®
SCANAMID 6 B12^ FX30 Polykemi AB Nylon 6 SCANAMID 6
Escorene™ Ultra MV 02528EH2 ExxonMobil Chemical EVA Escorene™ Ultra
LNP™ THERMOCOMP™ PF00C compound SABIC Innovative Plastics Nylon 6 LNP™ THERMOCOMP™