Category: | PVC, Rigid , Rigid Polyvinyl Chloride |
Manufacturer: | INEOS Compounds |
Trademark: | EVICOM™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | LXC2nx_EVICOM-RI5-011.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
The values listed for Tensile Modulus were tested at an unspecified rating. The values listed for Coefficient of Thermal Expansion were tested at an unspecified rating. The values listed for Thermal Conductivity were tested at an unspecified rating. |
General Information | |
---|---|
Features |
|
Appearance |
|
Forms |
|
Processing Method |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
Rockwell Hardness (R-Scale) | 115 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (23°C) | 2.80 | MPa | ASTM D638 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
CLTE - Flow | 6.0E-5 | cm/cm/°C | ASTM D696 |
Thermal Conductivity | 0.16 | W/m/K | ASTM C177 |
Additional Information |
---|
Vicat Softening Point, BS2782 120B: 63°C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Vi-Chem PVC VIR 6186 | Vi-Chem Corporation | PVC, Rigid | Vi-Chem PVC |
TPV Elastoprene® N90A-E | ELASTORSA Elastomeros Riojanos S.A. | PP+EPDM | TPV Elastoprene® |
Evoprene™ G 964 | AlphaGary | SEBS | Evoprene™ G |
Diamond HIPS HI-860 | Diamond Polystyrene | PS (HIPS) | Diamond HIPS |
Vyncolit® X7530 | SBHPP | Phenolic | Vyncolit® |