Category: | XLPE , Crosslinked Polyethylene |
Manufacturer: | Crosspolimeri S.p.A. |
Trademark: | GETILAN |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | LVzF5Z_GETILAN-ATP-130-XP.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
GETILAN ATP/130 XP is a crosslinkable polythene. GETILAN ATP/130 XP is a high density chemically crosslinkable polythene to produce relatively flexible hoses suitable for hydro-thermosanitary features and also for water conduction. It is a conveniently grafted polythene able to react in presence of moisture and of catalyst. We normally suggest our type MAC/100 PSF. REACTION BETWEEN GRAFTING AND CATALYST These two polythenes, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5 Certify: DIN 16892 |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.947 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 1.0 - 3.0 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D) | 59 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield) | 20.0 | MPa | IEC 60811 |
Tensile Strain (Break) | 370 | % | IEC 60811 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 120 | °C | ASTM D1525 |
Service Temperature | -60 - 100 | °C |
Additional Information | Nominal Value | ||
---|---|---|---|
Pressure Test | |||
95°C 1 | Pass | ||
95°C 2 | Pass |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 170 | °C | |
Cylinder Zone 2 Temp. | 180 | °C | |
Cylinder Zone 3 Temp. | 190 | °C | |
Cylinder Zone 4 Temp. | 205 | °C | |
Cylinder Zone 5 Temp. | 220 | °C | |
Die Temperature | 225 | °C |
Extrusion instructions |
---|
CROSSLINKING:Crosslinking of the finished product is obtained by: Immersion of the bobbin into hot water at 85/90°C for two hours (up to 3 mm thickness). Steam treatment at 0.15 bar for 5/6 hours. |
Note Message | |
---|---|
1 . | 1 hr, 4.8 MPa |
2 . | 1000 hr, 4.4 MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Michimid K4200MN40 | API Polymers, Inc. | Nylon 66 | Michimid |
Xuchuan XCW-8066L | Xuchuan Chemical (Suzhou) Co., Ltd | PUR, Unspecified | Xuchuan |
Argothane® 27303 | Argotec LLC | TPU, Unspecified | Argothane® |
Exxtral™ Performance Polyolefin BNT013 | ExxonMobil Chemical | TPO | Exxtral™ Performance Polyolefin |
LEXAN™ 940A resin | SABIC Innovative Plastics | PC | LEXAN™ |