| Category: | PVC, Flexible , Flexible Polyvinyl Chloride |
| Manufacturer: | Technovinyl Polymers India Ltd. |
| Trademark: | K-vinyl |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | LVlalX_K-vinyl-KSF-54.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
K-vinyl KSF-54 is a Flexible Polyvinyl Chloride material. It is available in Africa & Middle East. Typical applications include:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | ASTM D792 | ||
| -- 1 | 0.550 | g/cm³ | |
| -- | 1.16 | g/cm³ |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 54 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Abrasion Resistance - Volume Loss (130°C) 2 | -132 | mm³ | DIN 53516 |
| Aging | Nominal Value | Unit | |
|---|---|---|---|
| Heat Aging - Loss (130°C) 3 | 0.60 | % |
| Additional Information | Nominal Value | ||
|---|---|---|---|
| Slip Resistance | |||
| Dry | 0.620 | ||
| Wet | 0.560 | ||
| Specific Durability Index | 1.60 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | ASTM D412 | ||
| Yield 4 | 23.5 | MPa | |
| Yield | 13.2 | MPa | |
| Tensile Elongation | ASTM D412 | ||
| Break 5 | 220 | % | |
| Break | 430 | % |
| Note Message | |
|---|---|
| 1 . | After blowing |
| 2 . | 3 hrs |
| 3 . | 3 hrs |
| 4 . | After Heat Ageing at 100°C for 7 days |
| 5 . | After Heat Ageing at 100°C for 7 days |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Makrolon® WB1239 | Covestro - Polycarbonates | PC | Makrolon® |
| RTP 801 TFE 10 | RTP Company | Acetal (POM) Copolymer | RTP |
| POLIGOM G/30 C | Crosspolimeri S.p.A. | EPDM | POLIGOM |
| Infino WP-1100 | LOTTE ADVANCED MATERIALS CO., LTD. | PC+ABS | Infino |
| Styropek® BF 295 | Styropek S.A. de C.V. | PS (EPS) | Styropek® |