Sarlink TPV 24445N is a high performance thermoplastic vulcanizate used in a variety of consumer and industrial applications. Sarlink TPV 24445N is a medium hardness, low density, UV stabilized grade suitable for injection molding. |
General Information | |
---|---|
Features |
|
Uses |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.928 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 1.0 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 45 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Break) | 2.96 | MPa | ASTM D412 |
Tensile Elongation (Break) | 300 | % | ASTM D412 |
Legal statement |
---|
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries. |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 127 - 149 | °C | |
Middle Temperature | 138 - 160 | °C | |
Front Temperature | 149 - 171 | °C | |
Nozzle Temperature | 171 - 193 | °C | |
Processing (Melt) Temp | 171 - 193 | °C | |
Mold Temperature | 21 - 38 | °C | |
Injection Pressure | 1.38 - 5.52 | MPa | |
Back Pressure | 0.172 - 0.689 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C). |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MAZMID B 150 FV 50 | Mazzaferro Indústria e Comércio de Polímeros e Fibras Ltda. | Nylon 6 | MAZMID B |
Greenflex® FF 45 | Versalis S.p.A. | EVA | Greenflex® |
HiFill® PET GF/M40 BK | Techmer Engineered Solutions | PET | HiFill® |
Kepital® F30-03 | Korea Engineering Plastics Co., Ltd | Acetal (POM) Copolymer | Kepital® |
Hostacom EKC 133N C11376 | LyondellBasell Industries | PP Copolymer | Hostacom |