Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Teknor Apex Company (Chem Polymer) |
Trademark: | Chemlon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | KQ52mi_Chemlon-109-14-GH.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Chemlon 109-14 GH is an impact modified, 14% glass fibre filled, heat stabilised injection moulding grade of nylon 66. It is formulated to offer an excellent balance between impact strength and rigidity. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.20 | g/cm³ | ISO 1183 |
Water Absorption (Equilibrium, 23°C, 50% RH) | 1.8 | % | ISO 62 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 4700 | MPa | ISO 527-2 |
Tensile Stress | 105 | MPa | ISO 527-2 |
Tensile Strain (Break) | 4.0 | % | ISO 527-2 |
Flexural Modulus | 4000 | MPa | ISO 178 |
Flexural Stress | 130 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | 14 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | 75 | kJ/m² | ISO 179/1eU |
Notched Izod Impact | 13 | kJ/m² | ISO 180/A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, not annealed | > 240 | °C | ISO 75-2/B |
1.8 MPa, not annealed | 230 | °C | ISO 75-2/A |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Surface Resistivity | 1.0E+14 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+16 | ohms·cm | IEC 60093 |
Comparative Tracking Index | 500 | V | IEC 60112 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 2.0 | hr | |
Rear Temperature | 275 - 295 | °C | |
Middle Temperature | 275 - 295 | °C | |
Front Temperature | 275 - 295 | °C | |
Processing (Melt) Temp | 280 - 295 | °C | |
Mold Temperature | 80.0 - 90.0 | °C | |
Injection Rate | Fast | ||
Back Pressure | Low | ||
Screw Speed | Moderate |
Injection instructions |
---|
No drying is necessary unless the material has been exposed to air for longer than three hours. The appearance of splash marks on the surface of mouldings indicates excessive moisture is present. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 300 HF L UV | RTP Company | PC | RTP |
Braskem PP R7023-50NA | Braskem America Inc. | PP Random Copolymer | Braskem PP |
Crastin® BM6450XD BK560 | DuPont Performance Polymers | PBT | Crastin® |
Favorite LL051 | Favorite Plastics | LDPE+LLDPE | Favorite |
Starex TX-0520I | LOTTE ADVANCED MATERIALS CO., LTD. | MABS | Starex |