Andur 82 DGP/Curene® 442

Category: PUR-Ether/TDI , Polyurethane (Polyether, TDI)
Manufacturer: Anderson Development Company
Trademark: Andur
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: IpzA99_Andur-82-DGP-Curene-442.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Andur 82-DGP is a polyether (PTMG) based liquid, isocyanate terminated prepolymer. An elastomer with a hardness of 82 to 85 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combinations with Curene 442 and other diamines, or by the use of plasticizers.
General Information
Forms
  • Liquid
PhysicalNominal ValueUnitTest Method
Density 1.23g/cm³ASTM D1505
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D)83ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress (100% Strain)53.8MPaASTM D412
Tensile Strength (Yield)62.1MPaASTM D412
Tensile Elongation (Break)150%ASTM D412
Bayshore Resilience 45%ASTM D2632
ThermosetNominal ValueUnit
Pot Life 1.0 - 1.5min
Demold Time (100°C)5.0min
Post Cure Time (100°C)16hr
Additional Information
Durometer Hardness, ASTM D2240, Shore D: 80 to 85Die C Tear, ASTM D1004: 1375 pliAverage Split Tear, ASTM D1938: 315 pliStoichiometry Curative Level: 95%Mix Temperature: Andur 82 DGP: 140-180°F Curene 442: 250°F
Resin Grade Manufacturer Category Trademark
Stanyl® ForTii™ K12 DSM Engineering Plastics Nylon 4T Stanyl® ForTii™
Chemlon® 130 G BK200 Teknor Apex Company (Chem Polymer) Nylon 66 Chemlon®
Ferro PP TPP20AN73NA Ferro Corporation PP, Unspecified Ferro PP
Ferro PP TPP25AN96GY Ferro Corporation PP Copolymer Ferro PP
KRATON® D1101 E Kraton Polymers LLC SBS KRATON®