Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | RTP Company |
Trademark: | RTP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | InqLAG_RTP-ESD-A-201H.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Warning: The status of this material is 'Commercial: Limited Issue' The data for this material has not been recently verified. Please contact RTP Company for current information prior to specifying this grade. |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.23 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.18 mm) | 0.60 - 0.90 | % | ASTM D955 |
Water Absorption (23°C, 24 hr) | 1.0 | % | ASTM D570 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 4140 | MPa | ASTM D638 |
Tensile Strength | 65.5 | MPa | ASTM D638 |
Tensile Elongation (Break) | 2.0 | % | ASTM D638 |
Flexural Modulus | 3790 | MPa | ASTM D790 |
Flexural Strength | 93.1 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 91 | J/m | ASTM D256 |
Unnotched Izod Impact (3.18 mm) | 640 | J/m | ASTM D4812 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 216 | °C | ASTM D648 |
1.8 MPa, not annealed | 188 | °C | ASTM D648 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Surface Resistivity | 1.0E+6 | ohms | ASTM D257 |
Volume Resistivity | 1.0E+3 | ohms·cm | ASTM D257 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.59 mm, RTP Tested) | HB | UL 94 |
Additional Information |
---|
Mold Shrinkage, Linear-Flow, ASTM D955, 0.25in.: 12mil/in.Tensile Elongation, ASTM D638: 2-4%Volume Resistivity, ASTM D257: 10E3-10E6 ohm-cmSurface Resistivity, ASTM D257: 10E6-10E9 ohm/sq |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 274 - 293 | °C | |
Middle Temperature | 274 - 293 | °C | |
Front Temperature | 274 - 293 | °C | |
Mold Temperature | 65.6 - 93.3 | °C | |
Injection Pressure | 103 - 124 | MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PROTEQ™ C24UT4 | Marplex Australia Pty. Ltd. | PP Copolymer | PROTEQ™ |
SCANAMID 6 B12^FC | Polykemi AB | Nylon 6 | SCANAMID 6 |
4DUR® 9K22110 | 4Plas | PBT | 4DUR® |
ExxonMobil™ PP5722E1 | ExxonMobil Chemical | PP Homopolymer | ExxonMobil™ |
Grivory® GV-4H | EMS-GRIVORY | Nylon 66+Nylon 6I/X | Grivory® |