Hylon® N1013L

Category: Nylon 66 , Polyamide 66
Manufacturer: Ravago Manufacturing Americas, LLC
Trademark: Hylon®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: Iib2Gl_Hylon-N1013L.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Nylon 66, 13% Glass Filled
General Information
Filler / Reinforcement
  • Glass Fiber, 13% Filler by Weight
RoHS Compliance
  • RoHS Compliant
UL File Number
  • E157012
PhysicalNominal ValueUnitTest Method
Density 1.23g/cm³ISO 1183
Molding Shrinkage - Flow (3.18 mm)0.60 to 0.90%ISO 294-4
Water Absorption (23°C, 24 hr)1.0%ISO 62
MechanicalNominal ValueUnitTest Method
Tensile Stress (Break)118MPaISO 527-2
Tensile Strain (Break)2.5%ISO 527-2
Flexural Modulus 5000MPaISO 178
Flexural Stress 179MPaISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength 4.0kJ/m²ISO 180
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)235°CISO 75-2/A
FlammabilityNominal ValueTest Method
Flame Rating UL 94
    1.50 mm HB
    3.00 mm HB
Resin Grade Manufacturer Category Trademark
RTP 804 TFE 10 RTP Company Acetal (POM) Copolymer RTP
Restramid PA 6 50GF Polimarky Spolka Jawna Nylon 6 Restramid
Telcar® TL-6055 Teknor Apex Company TPE Telcar®
Eastar™ DN011 Eastman Chemical Company Copolyester Eastar™
LNP™ LUBRICOMP™ WFP36 compound SABIC Innovative Plastics PBT LNP™ LUBRICOMP™