Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | ResMart |
Trademark: | ResMart Ultra |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | IiZhIt_ResMart-Ultra-TPU-90A-ES.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Polyester based TPU Shore 90A hardness for injection molding or extrusion applications |
General Information | |
---|---|
Agency Ratings |
|
RoHS Compliance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.19 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 90 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 31.0 | MPa | ASTM D638 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Elongation (Break) | 440 | % | ASTM D412 |
Tear Strength | 115 | kN/m | ASTM D624 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature - Desiccant Dryer | 82.2 to 104 | °C | |
Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr | |
Suggested Max Moisture | 0.010 | % | |
Processing (Melt) Temp | 185 to 210 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sumitomo Epoxy E 2748-9641D | Sumitomo Bakelite North America, Inc. | Epoxy | Sumitomo Epoxy |
TAROPRENE® 1 A80 E1N | Taro Plast S.p.A. | TPV | TAROPRENE® |
DAI-EL™ G-701BP | DAIKIN AMERICA, INC. | Fluorelastomer | DAI-EL™ |
OP - PC/PEI 10GF | Oxford Polymers | PEI+PC | OP - PC/PEI |
OXPEKK® MG300 | Oxford Performance Materials, Inc. | PEKK | OXPEKK® |