Greenflex® FD 23

Category: EVA , Ethylene Vinyl Acetate Copolymer
Manufacturer: Versalis S.p.A.
Trademark: Greenflex®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: I7bybW_Greenflex-FD-23.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 represents the additivated version with slip and antiblocking of Greenflex FD 20.

Films produced from Greenflex FD 23 exhibit good optical properties, high impact resistance, tensile strength, elongation at break and low creep.

Main Application
Greenflex FD 23 is recommended for thermo-shrinkable films and multilayer stretch films for food packaging, included deep-frozen food packaging.
General Information
Additive
  • Antiblock
  • Slip
Features
  • Antiblocking
  • Copolymer
  • Food Contact Acceptable
  • Good Creep Resistance
  • High Elongation
  • High Impact Resistance
  • High Tensile Strength
  • Opticals
  • Slip
Uses
  • Film
  • Food Packaging
  • Multilayer Film
  • Shrink Wrap
  • Stretch Wrap
Agency Ratings
  • EU Food Contact, Unspecified Rating
Forms
  • Pellets
Processing Method
  • Blown Film
PhysicalNominal ValueUnitTest Method
Density 0.924g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)0.50g/10 minISO 1133
Vinyl Acetate Content 5.0wt%Internal Method
HardnessNominal ValueUnitTest Method
Shore Hardness ISO 868
    Shore A, Injection Molded 95
    Shore D, Injection Molded 44
MechanicalNominal ValueUnitTest Method
Coefficient of Friction (vs. Itself - Dynamic, Blown Film)> 0.20ISO 8295
FilmsNominal ValueUnitTest Method
Film Thickness - Recommended / Available 50 to 200µm
Tensile Modulus ISO 527-3
    1% Secant, MD : Blown Film 120MPa
    1% Secant, TD : Blown Film 125MPa
Tensile Stress ISO 527-3
    MD : Yield, Blown Film 8.00MPa
    TD : Yield, Blown Film 8.00MPa
    MD : Break, Blown Film 25.0MPa
    TD : Break, Blown Film 25.0MPa
Tensile Elongation ISO 527-3
    MD : Break, Blown Film 450%
    TD : Break, Blown Film 600%
Dart Drop Impact 1(Blown Film)420gISO 7765-1
Elmendorf Tear Strength 2ISO 6383-2
    MD 26.0kN/m
    TD 40.0kN/m
ThermalNominal ValueUnitTest Method
Brittleness Temperature < -80.0°CASTM D746
Vicat Softening Temperature 85.0°CISO 306/A
Melting Temperature 104°CInternal Method
OpticalNominal ValueUnitTest Method
Gloss (45°, Blown Film)72ASTM D2457
Haze (Blown Film)8.0%ISO 14782
ExtrusionNominal ValueUnit
Melt Temperature 170 to 200°C
Note Message
1 .F50
2 .Blown Film
Resin Grade Manufacturer Category Trademark
Maxelast® P1860D Nantong Polymax Elastomer Technology, Co., Ltd TPE Maxelast®
ResMart Ultra PBT 10 ResMart PBT ResMart Ultra
Sylvin 6201-75 Natural Sylvin Technologies Incorporated PVC, Unspecified Sylvin
Zytel® RS LC4601 NC010 DuPont Performance Polymers Nylon, Unspecified Zytel® RS
OTECH PVC OM6037 - Gasket OTECH Corporation PVC, Unspecified OTECH PVC