Sumikon®EME-6650RM is an epoxy; Epoxy resin products,. It can be processed by encapsulation and is available in North America. |
General Information | |
---|---|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.95 | g/cm³ | ASTM D792 |
Water Absorption (24 hr) | 0.22 | % | ASTM D570 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Flexural Modulus (25°C) | 18600 | MPa | ASTM D790 |
Flexural Strength (25°C) | 157 | MPa | ASTM D790 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | 165 | °C | ASTM E1356 |
Thermal Conductivity | 0.75 | W/m/K | ASTM C177 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 5.0E+13 | ohms·cm | ASTM D257 |
Thermoset | Nominal Value | Unit | |
---|---|---|---|
Demold Time (175°C) | 0.75 - 1.3 | min | |
Post Cure Time (175°C) | 1.0E-4 - 8.0 | hr |
Additional Information |
---|
Spiral Flow, SB-U-03-003: 110 cmGel Time, SB-U-03-005, 175°C: 34 secThermal Expansion, SB-U-02-002, T |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 207D TFE 15 | RTP Company | Nylon 612 | RTP |
Sumitomo Epoxy E 2748-9641D | Sumitomo Bakelite North America, Inc. | Epoxy | Sumitomo Epoxy |
Sylvin 9077-90 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Ferro PP RPP10GT25UL | Ferro Corporation | PP, Unspecified | Ferro PP |
Padermid 6 AF | TKC Kunststoffe e.K. | Nylon 6 | Padermid |