NANCAR® 3345

Category: NBR , Acrylonitrile Butadiene Rubber
Manufacturer: Nantex Industry Co., Ltd.
Trademark: NANCAR®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: HihSmL_NANCAR-3345.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
NANCAR® 3345 is a medium high acrylonitrile butadiene copolymer with good oil resistance. It is polymerized at low temperature and contains sufficient antioxidant for normal aging conditions. It has low Mooney viscosity, superior processing characteristics, fast curing rate, low mold fouling, superior resilience properties and superior flowability.

NANCAR® 3345 is an excellent multi-purpose nitrile elastomer. It may be blended with vinyl resins to produce smooth extrusions and nerve-free sheets. Suggested applications include those in fuel hoses, packings, gaskets, oil seals, other car parts, oil resistant belts, footwear, roll covers and sponge products.
General Information
Additive
  • Antioxidant
Features
  • Antioxidant
  • Copolymer
  • Good Flow
  • Good Processability
  • Low Viscosity
  • Oil Resistant
Uses
  • Automotive Applications
  • Belts/Belt Repair
  • Footwear
  • Gaskets
  • Hose
  • Seals
  • Sheet
Forms
  • Pellets
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.980g/cm³
Mooney Viscosity (ML 1+4, 100°C)45MUASTM D1646
Acrylonitrile Content - Bound 33.0%Internal Method
Solubility - in MEK 100%
Stabilizer Non-staining
ThermalNominal ValueUnitTest Method
Heat Loss 0.20%ASTM D5688
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shore A 174
    Shore A 273
    Shore A 372
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    300% Strain 49.41MPa
    300% Strain 510.4MPa
    300% Strain 611.1MPa
Tensile Strength ASTM D412
    Yield 726.0MPa
    Yield 825.7MPa
    Yield 926.9MPa
Tensile Elongation ASTM D412
    Break 10650%
    Break 11590%
    Break 12570%
Tear Strength 61.8kN/mASTM D624
Compression Set 13(100°C, 70 hr)59%ASTM D395
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air 14(100°C, 70 hr)-3.0%ASTM D865
Change in Ultimate Elongation in Air 15(100°C, 70 hr)-27%ASTM D865
Change in Durometer Hardness in Air 16(Shore A, 100°C, 70 hr)4.0ASTM D865
Change in Tensile Strength 17ASTM D471
    100°C, 70 hr, in ASTM #1 Oil -2.0%
    100°C, 70 hr, in ASTM #3 Oil -30%
Change in Ultimate Elongation 18ASTM D471
    100°C, 70 hr, in ASTM #1 Oil -21%
    100°C, 70 hr, in ASTM #3 Oil -29%
Change in Durometer Hardness 19ASTM D471
    Shore A, 100°C, 70 hr, in ASTM #1 Oil 0.0
    Shore A, 100°C, 70 hr, in ASTM #3 Oil -10
Change in Volume 20ASTM D471
    100°C, 70 hr, in ASTM Oil #1 0.20%
    100°C, 70 hr, in ASTM Oil #3 15%
Note Message
1 .Cured for 60.0 min at 150°C
2 .Cured for 40.0 min at 150°C
3 .Cured for 20.0 min at 150°C
4 .Cured for 20.0 min at 150°C
5 .Cured for 40.0 min at 150°C
6 .Cured for 60.0 min at 150°C
7 .Cured for 60.0 min at 150°C
8 .Cured for 40.0 min at 150°C
9 .Cured for 20.0 min at 150°C
10 .Cured for 20.0 min at 150°C
11 .Cured for 40.0 min at 150°C
12 .Cured for 60.0 min at 150°C
13 .Cured for 60.0 min at 150°C
14 .Cured for 40.0 min at 150°C
15 .Cured for 40.0 min at 150°C
16 .Cured for 40.0 min at 150°C
17 .Cured for 40.0 min at 150°C
18 .Cured for 40.0 min at 150°C
19 .Cured for 40.0 min at 150°C
20 .Cured for 40.0 min at 150°C
Resin Grade Manufacturer Category Trademark
Maxxam™ ET5200-8016 RS Natural PolyOne Corporation PP, Unspecified Maxxam™
Elastron® TPO T100.D42.N Elastron USA, Inc. TPO (POE) Elastron® TPO
Enviramid® N2330STHL BK Ravago Manufacturing Americas, LLC Nylon 6 Enviramid®
KumhoSunny ASA XC200 Shanghai KumhoSunny Plastics Co., Ltd. ASA KumhoSunny ASA
Pibiflex® RFB40011 NERO SO.F.TER. SPA TPC-ET Pibiflex®